According to the official regulation EN ISO 3146, polymers do usually not have a sharp melting point as known for low-molecular substances. Here, we demonstrate the feasibility to employ the M-565 for the melting range determination of semi-crystalline polymers by capillary tube method according to EN ISO 3146.
Semi-crystalline poly(tetrafluoroethylene) (PTFE was chosen as test compound for the melting range measurements. For the analysed PTFE samples, we report a narrow melting range between 322.9 ± °C and 326.0 ± 0.1 °C.
With the M-565 the melting process can be measured and recorded without modification of the instrument

Atsisiųsti programą Atsisiųsti programą Į programos apžvalgą Susisiekite su mumis

Application Download Form

* Šie laukai yra privalomi.

** Atkreipkite dėmesį, kad jūsų asmeniniai duomenys bus saugomi saugiai ir laikantis BDAR (ES) 2016/679 dėl asmenų apsaugos ryšium su asmens duomenų tvarkymu ir laisvo tokių duomenų judėjimo. Turite teisę prašyti iš mūsų gauti visus jūsų saugomus asmeninius duomenis, ištaisyti, ištrinti ar apriboti asmens duomenų tvarkymą ir bet kuriuo metu atsiimti savo sutikimą. Asmens duomenys nebus perduodami už mūsų įmonių grupės ribų, nei parduodami kitoms įmonėms. Asmens duomenys gali būti naudojami rinkodaros ir bendravimo tikslams, kol sutikimas bus atšauktas.

Rodyti daugiau programų:

Analitika

Žiūrėti daugiau programų, susijusių su:

Matavimo įranga